You really must be good with your hands unless you want to pay someone to do everything for you.
Repair boat floor rot. Fiberglass boat flooring replacement is a common procedure that a lot of boat aficionados perform to restore their boats and keep them in good shape after years of use flooring can get damaged particularly if left exposed to all weather conditions for a long time. Therefore you should consider working on your own boat. With a boat floor made out of wood dry rot will be one of the primary problems you have to deal with. Therefore it will need replacing.
Owning a boat means that you re going to run into problems at some point or another. You cannot repair the boat floor while rotten wood remains as it will only continue to rot. I used git rot to repair the delaminated hulls on my 1982 hobie cat 16 sailboat. A clean professional repair in progress by one of our customers.
Having repair work completed on your boat can be expensive. Boat floor repair dry rot. A rotted floor is one of. Penetration capillary action is the principal on which git rot works.
But if you buy a fixer upper or have an older boat you love and don t want to part with there s a fair chance you ll need to replace part or all of the rotten boat. Replacing a rotten boat deck is a fairly common task and it s a lot easier than you might think. Hopefully when you bought your boat you gave it a thorough pre purchase inspection and didn t get any nasty surprises. Add thin strips of wood under the edges of the repair patch to make it flush with the floor of the boat.
First acquire a git rot kit for yourself. New flooring was installed. Holes left by drilling may be filled with a mixture of dry saw dust and git rot or a marine repair epoxy compound. Therefore the most expedient way to apply the git rot is into the end grain of the wood wherever possible.
Replace the carpet or use a fiberglass repair kit to finish the surface of the floor. This is especially effective on loose wood and end grain materials that might be exposed. Needed 5 quarts so this was an expensive fix. Example of transom stringer repair.
Where the wood was weak the stringer was saturated with cpes and layup laminating resin through drilled holes. The length of the wood screws is equal to the combined thickness of the floor and the marine plywood. This kit includes a two part liquid epoxy that soaks into wood via capillary action.